伊利石型含钒石煤无添加剂焙烧-酸浸提钒工艺研究

    Study on extracting vanadium by no additive roasting-acid leaching from a illite-type vanadium-containing stone coal

    • 摘要: 以陕西商洛某伊利石型石煤钒矿为原料,采用无添加剂焙烧-酸浸法从石煤中提取钒,分析了焙烧温度、焙烧时间及浸出温度、硫酸浓度、浸出时间、液固比对钒浸出率的影响。结果表明,焙烧温度对钒的浸出率有显著影响,焙烧温度过低和过高,钒都难以被浸出, 只有在适当焙烧温度范围内,钒的浸出效果较好。以850 ℃条件下焙烧2 h后的石煤焙烧料,在硫酸浓度5%、浸出温度90 ℃、浸出时间1 h、液固比4∶1 mL/g的条件下,钒浸出率达72.53%,表明伊利石型含钒石煤采取无添加剂焙烧提钒是可行的。浸渣样品的SEM分析结果表明,石煤焙烧过程中生成的钒包裹体和部分未从伊利石中释放的钒是造成钒损失的主要原因。

       

      Abstract: The illite-type stone coal containing vanadium from the Shangluo region of Shaanxi province is selected as raw materials.Vanadium is extracted by no additive roasting-acid leaching, the effects of roasting time, roasting time, and leaching temperature, leaching time, sulfuric acid concentration, liquid to ratio are investigated.The results show that roasting temperature has a significant influence on leaching rate of vanadium recovery.It is difficult to leach vanadium at the condition of lower and higher roasting temperature, and only when roasting temperature is within proper temperature range, the leaching effect of vanadium is better.It is feasible to extract vanadium from illite-type stone coal containing vanadium by additive-free roasting process,under the conditions that roasting temperature remains at 850 ℃ for 2 h, the sulfuric acid concentration is 5%,the leaching temperature remains at 90 ℃ for 1 h, and the liquid-solid ratio of 4∶1 mL/g, the leaching rate of vanadium is 72.53%.The results of SEM analysis show that the main reasons for the loss of vanadium are the produced vanadium inclusions in the roasting process and the vanadium which is not released from the illite.

       

    /

    返回文章
    返回