安徽铁尾矿浮选回收云母试验研究

    Experimental study on mica recovery from iron tailings by flotation in Anhui Province

    • 摘要:

      安徽某铁尾矿中云母含量较高,具有一定的综合回收价值。尾矿中K2O含量为1.21%,金属矿物主要为残余的赤(镜)铁矿,非金属矿物主要为石英、云母、白云石、绿泥石等。其中,云母主要为白云母,少量黑云母,白云母主要以单体形式存在,少量为连生体,嵌布粒度粗细不均,最大粒径可达0.650 mm,主要分布在0.050~0.200 mm之间。矿物学研究表明,影响云母回收的主要因素是层状硅酸盐矿物,绿泥石含量较高,在云母浮选过程中易进入精矿,从而影响云母精矿的品质。根据该尾矿特性,本文应用浮选工艺进行了云母回收试验研究,在碱性矿浆环境下,不磨矿直接浮选,采用BK500新型调整剂,BK421D和混合胺分别作阴离子和阳离子捕收剂,通过“一粗一扫四精,中矿顺序返回”的浮选工艺流程,闭路试验获得了产率为9.77%、K2O含量为7.89%、回收率为64.41%的云母精矿,取得了良好的选矿指标。研究结果为该铁尾矿资源化利用奠定了技术基础。

       

      Abstract:

      The content of mica in an iron tailings in Anhui is relatively high, which has certain comprehensive recovery value.The content of K2O in iron tailings is 1.21%, and the main metal minerals are residual hematite (specularite), and the main non-metallic minerals are quartz, mica, dolomite, chlorite, etc.Among them, mica is mainly muscovite and a little biotite.Muscovite mainly exists in the form of monomer, and a small amount of muscovite is connected.The particle size of muscovite is uneven, the maximum particle size can reach 0.650 mm, and the main distribution is between 0.050-0.200 mm.The mineralogical study shows that the main factor affecting the recovery of mica is the high content of chlorite, which is easy to enter the concentrate during the flotation process of mica, thus affecting the quality of mica concentrate.According to the characteristics of the tailings, in the alkaline pulp environment, BK500 is used as regulator, and BK421D and mixed amine are used as anionic and cationic collectors respectively in tests.Through the flotation process of “one rough, one sweep and four fine, middling ore return in sequence”, and mica concentrate is obtained with yield of 9.77%, K2O grade of 7.89% and recovery of 64.41%.The research results lay a technical foundation for the resource utilization of the iron tailings.

       

    /

    返回文章
    返回