Abstract:
The oxidation rate of a lead and zinc mult-metal oxidation mineral is 56.30% and 93.9%.The index of sulfuration lead of concentrate yield rate being 7.65%, Pb grade being 61.00%、Pb recovery being 43.82% sulfuration lead, oxidation lead of concentrate yield being 10.15%, Pb grade being 51.41%, Pb recovery being 49.00%, oxidation zinc of concentrate yield being 23.22%, Zn grade being 45.77%, Zn recovery being 85.02% was got on the condition of the flowsheet of shaking table separate, regringing and flotating table concentrate and directness flotating table tailing, flotation flowsheet being sulfuration lead priority flotation of sulfuration lead, oxidation lead and oxidation zinc in turn.