用振动高梯度磁选精选界牌高岭土的研究

    STUDY ON THE PURIFICATION OF JIEPAI KAOLINE BY VIBRATING HGMS

    • 摘要: 本文详细研究了各种因素对湖南界牌高岭土(Fe2O3+TiO2>0.85%)高梯度磁选除铁、钛效果的影响。试验表明,界牌高岭土经一次高梯度磁选,可获得产率大于85%,Fe2O3+TiO2小于0.5%的一级产品,白度可从入选前的61.3%提高到70.3%;该产品经进一步精选,Fe2O3+TiO2可降到0.4%以下。

       

      Abstract: The problem to remove iron and titanium contaminantions from kaoline has still need to besolved pressingly in ceramic industry in China. In this paper, it is studied that various factors influenceon the efficiency of removing iron and titanium from Jiepai kaoline (Fe2O3+TiO2,>0. 85%)by meansof vibrating high-gradient magnetic separation (HGMS). The results showed that Kaoline productcontaining minus 0. 5% of (Fe2O3+TiO2) was produced with its yeild of plus 85% and its whitenesswas improved from 61. 3% to 70.3% after separating. But, the total content of (Fe2O3 +TiO2) can bedecreased to minus 0. 4% after cleaning.

       

    /